Technical Data for Advapoder
 Nano and Submicron Diamond Powder
Crystal Monocrystal
Crystal Shape Cubic Hexahedron, Cubic Octahedron
Type of Crystal Lattice Sphalerite Structure
Size Designation M0-0.10(um) / M0-0.25(um)
Paticle Size Distribution 0-0.20(d97) / 0-0.50(d97)
Specific Surface(m2/g) 108m2 / 50m2
Appearance Black Powder / Grey Powder
Bulk Weight(g/cm3) 3.2 ~ 3.45
Vickers Diamond Hardness 10000
Space Group Cubic Fd3m - O
Crystal Lattice Constant/nm 0.356696±0.000005
Neighbour Atom Space/nm 0.154
Coordination Isomerism 4
Atom Number in Unit Volume  1.77X1023
Interplanar Crystal(Synthetic) {111},{100}》{110},{113}
Interplanar Crystal(Natural) {111},{110}》{100}
Corrosion Resistance To resit any acid and be eroded in melted alkali.
Stable Temperature Range (Air) ~600℃
Stable Temperature Range (Vacuum) ~1700℃
Elasticity Modulus of Deformable Body/Gpa 44~54
Young's Modulus/Gpa 90~100
Molar Heat Capacity/(J/mol·K) 150K-1.0,298K-6.1,400K-10.6
Debye Temperature/K 0K-2220±20,0-800℃-1860±10
Heat Conductance/(W/m·K) 298K- ~2000,77K- ~17500
Velocity of Sound(m/s) 18000
Refractive Index(5900 Angstrom) 2.41
Transmission Wave Band(um) 0.225 - Far-infrared
Dielectric Constant 5.7
Dielectric Intensity(volt/cm) 107 (v/cm)
linear Expansion(K-1) 20~100℃ - 1.34X10-6
  20~400℃ - 2.29X10-6
  20~800℃ - 3.14X10-6
Solid-Solution Impurity Concentration N - Substitution (≤4.59X1019), Sheet (≤4.5X1020)
  B - Replacement(≤4.59X1019)
Band-gap Width/eV (Direct Band-gap) ~7.0(K=0)
                  (Indirect Band-gap) 5.470±0.005
Effective Quality (Cavity) ~1.0m0 0.25m0
                  (Electron) ~0.2m0 0.2m0
Mobility(cm2/V·s)(Cavity) 1550(Maximum)1200
                    (Electron) 2800(Maximum)1800
Polarizability 5.68±0.03